Plastering is applying a layer of mortar, usually cement and sand, over brick or block walls and concrete ceilings. It protects masonry from weather, hides joints and uneven surfaces, and gives a smooth base for putty and paint. External plaster is thicker and often done in two coats to keep rain out; internal plaster is thinner and finished smooth.
Also known as: cement plaster, rendering (external), wall plaster.
Quick facts
| Standard | IS 1661 (cement and cement-lime plaster finishes) |
| Typical thickness | Internal walls ~12 mm, external walls ~18–20 mm (often two coats), ceilings ~6–10 mm |
| Sand | P-sand or fine river sand |
| Alternatives | Gypsum plaster (internal), sand-faced plaster (external texture) |
| Curing | Keep moist for several days after application |
Plastering explained
Good plaster starts before the mortar is mixed. The wall should be cleaned and wetted, concrete surfaces should be hacked for grip, electrical and plumbing chases should be filled, and mesh should be fixed where masonry meets columns and beams. Masons then fix small mortar “dots” to set the thickness and line, and use an aluminium straight edge to keep walls flat and vertical.
Thicker is not better. Very thick plaster, used to hide crooked brickwork, tends to crack and come loose. Too much cement causes shrinkage cracks; too little makes plaster weak and dusty. After application, plaster must be cured. Most plaster defects — cracks, hollow-sounding patches, peeling paint — trace back to poor sand, no curing or skipped preparation. See plaster hollowness.
How buyers get cheated
- Thickness padding. Extra-thick plaster to hide bad masonry, sometimes billed as extra work. Check walls are straight before plastering.
- Dusty sand. Leads to cracks and powdery walls. Check the sand before work starts.
- No mesh at joints. Guarantees cracks at column-wall junctions. Look for mesh before plaster goes on.
- No curing. Insist on spraying for the agreed number of days.
Related terms
P-sand · Gypsum plastering · Sand-faced plaster · Chicken mesh at joints · Surface hacking · Plaster hollowness · Wall putty
Go deeper
Frequently asked questions
What is the difference between internal and external plaster?
External plaster faces rain and sun, so it’s thicker, often two coats, and sometimes includes a waterproofing additive. Internal plaster is thinner and finished smoother for putty and paint.
Why does new plaster crack?
Common causes are too much cement, dusty sand, too thick a layer, no mesh at concrete-masonry joints, and lack of curing. Fine hairline cracks are usually cosmetic; wide or growing cracks need an engineer’s look.
When can I paint after plastering?
Plaster needs to cure and then dry out. Painters often wait several weeks for new cement plaster; check the paint manufacturer’s recommendation.
Review and sources
- IS 1661, Code of Practice for Application of Cement and Cement-Lime Plaster Finishes
- IS 1542, Sand for Plaster — Specification